1. A dedicated person must be responsible for preparing polymer mortar to ensure the mixing quality.

2 Oz Chopped Strand Mat

2. Open the lid of the bucket by rotating it counterclockwise, and use a stirrer or other tools to re-stir the adhesive to avoid separation of the adhesive. Stir appropriately to avoid quality problems.
3. The mixing ratio of polymer mortar is: KL binder: 425# sulfoaluminate cement: sand (use 18 Fiber Glass sieve bottom): =1:1.88:3.25 (weight ratio).
4. Weigh the cement and sand in a measuring bucket and pour them into the iron ash tank for mixing. After stirring evenly, add the binder according to the mixing ratio and stir. The stirring must be even to avoid segregation and porridge-like appearance. Water can be added appropriately according to the workability.
5. Water is used for concrete.
6. Polymer mortar should be prepared as needed. It is best to use up the prepared polymer mortar within 1 hour. Polymer mortar should be placed in a cool place to avoid sunlight exposure.
7. Cut the Fiber Glass from the entire roll of fiberglass Fiber Glass according to the required length and width, leaving the necessary overlap length or overlap length.
8. Cut in a clean and flat place. The cutting must be accurate. The cut Fiber Glass must be rolled up. Folding and stepping are not allowed.
9. Make a reinforcement layer at the sun corner of the building. The reinforcement layer should be attached to the innermost side, 150mm on each side.
10. When applying the first coat of polymer mortar, the EPS board surface should be kept dry and harmful substances or impurities in the board cotton should be removed.
11. Scrape a layer of polymer mortar on the surface of the polystyrene board. The scraped area should be slightly larger than the length or width of the glass yarn, and the thickness should be about 2mm. Except for those with hemming requirements, polymer mortar is not allowed to be applied. On the side of the polystyrene board.
12. After scraping the polymer mortar, the grid should be arranged on it, with the curved surface of the grid facing the wall, and smooth application from the center to the surroundings so that the grid is embedded in the polymer mortar and the grid is not It should be wrinkled, and after the surface is dry, apply a layer of polymer mortar on it with a thickness of 1.0mm. The glass yarn should not be exposed.
13. The overlapping length around the glass yarn shall not be less than 70mm. At the cut parts, Fiber Glass patching shall be used to overlap, and the overlapping length shall not be less than 70mm.
14. A reinforcing layer should be made around the doors and windows, and the glass yarn of the reinforcing layer should be affixed to the innermost side. If the distance between the outer skin of the door and window frame and the surface of the base wall is greater than 50mm, the glass yarn should be affixed to the base wall. If it is less than 50mm, it needs to be turned over. The glass yarn laid on the large wall should be embedded in the outside of the door and window frames and glued firmly.
15. At the four corners of the door and window, after the standard net is applied, add a piece of 200mm×300mm standard net on the four corners of the door and window, place it at an angle of 90 degrees to the bisector of the window corner, and stick it on the outermost side for reinforcement; Add a piece of Fiber Glass 200mm long and standard width to the window at the inner corner, and attach it to the outermost side.
16. Below the first floor window sill, in order to prevent damage caused by impact, the reinforced glass yarn should be installed first, and then the standard glass yarn should be installed. Strengthen the connection between Fiber Glass.
17. The construction method for installing the reinforcement layer is the same as that of the standard glass yarn.
18. The glass yarn pasted on the wall should cover the folded glass yarn.
19. The glass yarn is applied from top to bottom. During simultaneous construction, the reinforced glass yarn is applied first, and then the standard glass yarn is applied.
20. After the glass yarn is glued, it should be prevented from being washed away or hit by rain. Protective measures should be taken for doors and windows that are prone to collision. Anti-pollution measures should be taken for the feeding port. Surface damage or pollution must be dealt with immediately.
21. The protective layer cannot be exposed to rain within 4 hours after construction.
22. After the protective layer is finally set, spray water for maintenance in a timely manner. When the average day and night temperature is higher than 15°C, it shall not be less than 48 hours, and when the average temperature of day and night is lower than 15°C, it shall not be less than 72 hours.
Contact Us

Author:

Mr. Lv Qingtao

Phone/WhatsApp:

15870567810

Popular Products
You may also like
Related Categories

Email to this supplier

Subject:
Email:
Message:

Your message must be betwwen 20-8000 characters

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send